ASME A333 Pipe
ASTM A333 is a specification that covers seamless and welded steel pipes designed for low-temperature service. These pipes are used in a wide range of industrial applications where low-temperature conditions are a concern.
Cryogenic Applications: ASME A333 piping is specifically designed for cryogenic applications where temperatures can be as low as -150 degree F (-101 degree ). They are commonly used in industries such as oil and gas, petrochemical, and power generation where low temperatures may be encountered during transportation and processing.
Coatings: ASME A333 pipe is available with a variety of coatings, hot-dip galvanized coatings, or other anti-corrosion coatings, depending on the application and environmental conditions.
Seamless and Welded: ASME A333 tubing is available in both seamless and welded forms. Seamless tubing is preferred for low-temperature applications because seamless tubing does not have welded seams, which are prone to cracking in extreme cold environments.
|
1 Ton, more quantity price will be lower |
|
|
ASME A333 pipe |
|
|
18.0mm-812.0mm or as required |
|
|
1.0mm-120.0mm or as required |
|
|
3m, 5.8m, 6m, 11.8m, 12m or as required |
|
|
Hot rolled, Cold rolled, Cold -drawing |
|
|
Control with in the standard, OD: plus /-1 percent , WT: plus /-5 percent |
|
|
Black painting, anti-corrosion oil, galvanized or as per required by customer |




1.Q: Are you a manufacturers and what is your production capacity?
2.Q: How many specifications does the product have and does it supportcustomization?
3.Q.How do you guarantee the quality of your products?
Popularne oznake: asme a333 pipe, China asme a333 pipe manufacturers, suppliers, factory