10# LSAW Welded Steel Pipe

Aug 09, 2023

10# LSAW Welded Steel Pipe

10# LSAW steel pipe is a high quality, durable and versatile solution for a variety of industrial applications. Manufactured from "10#" steel using the Longitudinal Submerged Arc Welding (LSAW) process, the pipe provides excellent strength and reliability for fluid transportation, structural support and more.

  10# LSAW Welded Steel Pipe

Q215-A, Q235-A, Q275-A, 10#-50#
According to customer requirements (inventory length 6M-12M)
5.54-12.7mm
610-1219mm
Bare, painting black, anti-corrosion

10# LSAW Welded Steel Pipe

 
300 MPa
450 MPa
25 percent
150
60 J/cm²
200 GPa
0.3


Grade: 10# (low carbon structural steel)